·POSITION:ApplicationCommon Question → When acetoxy cross-linking agents are used to make acetoxy sealant, a strong odor is released, and even symptoms of eye smoke may occur.

Why do bulges and blisters appear during the application of alkoxy sealant? How to reduce and avoid this phenomenon?
Date:2023/8/2 14:58:15  View:  【 Font Size:Big Medium Small 】  【CLOSE

There are two main reasons for the bubbling phenomenon of alkoxy sealant: internal and external.

1. External reasons: caused by application conditions. The main reason is that the temperature difference is too large or the construction surface temperature is too high.

2. Internal reasons: caused by alkoxy sealant itself. Because alkoxy sealant releases methanol during the curing process, and the boiling point of methanol is low, so when the construction surface temperature is too high, the released methanol cannot be volatilized in a timely and effective manner, it will vaporize inside the sealant and form bulges and bubbles.


The phenomenon that alkoxy sealant is easy to bubbling has not been completely solved. According to the vulcanization mechanism of this product, commonly used methods in the industry to reduce or decrease bubbling include:

1. Control the dosage of cross-linking agent, because the more cross-linking agent is added, the greater amount of methanol released and the easier it is to bubble.

2. Reduce the tack free time of the sealant so that the released methanol can have sufficient time to evaporate.

3. Use methanol absorbent. No good absorbent has been found yet.

4. Mainly avoid exposure to the sun during application


Font Size:Big Medium Small 】【CLOSE
Prev:Why is the storage stability of alkoxy sealant relatively poor?
Next:When acetoxy cross-linking agents are used to make acetoxy sealant, a strong odor is released, and even symptoms of eye smoke may occur.

Wechat

Wechat

Website

Website


Copyright © 2023 Hubei BlueSky New Material INC.
鄂ICP备05028071号 鄂公网安备 42900402000406号 网络经济主体信息湖北工商网监

 Home  Tel  Product
Trade
Hotline
+86-020-38856806
Head
Hotline
+86-020-38856809
WeiXin
Code
Wechat

Wechat

^
TOP